We emphasize progress and introduce new solutions into the market each year for Underground Gas Line , Fbe Coated Pipe Suppliers , Steel Pipe Industry , To learn more about what we can do for you, contact us at any time. We look forward to establishing good and long-term business relationships with you.
High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral Detail:

Product Description

Cangzhou Spiral Steel Pipes Group Co., Ltd have 4 production lines of anticorrosion & thermal insulation to perform the 3LPE coating and FBE coating. The maximum outside diameter can be 2600mm.

The coatings are suitable for the protection of buried or submerged steel pipes at design temperatures of -40℃ to +80℃.

The present standard specifies requirements for coatings that are applied to spirally welded steel pipes and fittings used for the construction of pipelines for conveying liquids or gases.

Applying this standard ensures that the PE coating provides sufficient protection against the mechanical thermal and chemical loads occurring during operation, transport, storage and installation.

Extruded coatings comprise three layers: an epoxy resin primer, a PE adhesive and an extruded polyethylene outer layer. The epoxy resin primer is applied as a powder. The adhesive can be applied either as a powder or by extrusion. For extruded coatings a differentiation is made between sleeve extrusion and sheet extrusion. Sintered polyethylene coatings are single or multi-layer systems. The polyethylene powder is fused onto the pre-heated component until the desired coating thickness is reached.

Epoxy resin primer

The epoxy resin primer is to be applied in powder form. The minimum layer thickness is 60μm.

PE adhesive

The PE adhesive can be applied in powder form or extruded. The minimum layer thickness is 140μm. the peel strength requirements vary depending on whether the adhesive was applied as a powder or was extruded.

Polyethylene coating

The polyethylene coating is applied either by sintering or by sleeve or sheet extrusion. The coating is to be cooled after application to avoid unwanted deformation during transport. Depending on the nominal size, there are different minimum values for the normal total coating thickness. In the case of increased mechanical loads the minimu layer thickess shall be increased by 0.7mm. minimum layer thickness are given in table 3 below.

product-description1


Product detail pictures:

High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral detail pictures

High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral detail pictures

High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral detail pictures


Related Product Guide:

We support our prospective buyers with ideal top quality merchandise and superior level provider. Becoming the specialist manufacturer in this sector, we have now attained abundant practical expertise in producing and managing for High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral , The product will supply to all over the world, such as: Tajikistan, Benin, Argentina, We can give our clients absolute advantages in product quality and cost control, and we have full range of molds from up to one hundred of factories. As product updating fast, we succeed in developing many high quality products for our clients and get high reputation.
  • The sales manager has a good English level and skilled professional knowledge, we have a good communication. He is a warm and cheerful man, we have a pleasant cooperation and we became very good friends in private.
    5 Stars By Rose from Iraq - 2017.06.25 12:48
    In China, we have many partners, this company is the most satisfying to us, reliable quality and good credit, it is worth appreciation.
    5 Stars By ROGER Rivkin from Adelaide - 2017.05.02 11:33
    Write your message here and send it to us