High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard – Spiral

Short Description:


Product Detail

Product Tags

Related Video

Feedback (2)

No matter new customer or previous client, We believe in prolonged time period and trustworthy relationship for Gas Lines , China Pipe Line Construction , Spiral Welded Steel Pipe , We sincerely hope to provide you and your company with a great start. If there is anything we will do to suit your needs, we shall be additional than pleased to do so. Welcome to our manufacturing facility for stop by.
High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard – Spiral Detail:

Physical properties of epoxy powder materials

Specific gravity at 23℃: minimum 1.2 and maximum 1.8
Sieve analysis: maximum 2.0
Gel time at 200 ℃: less than 120s

Abrasive blast cleaning

Bare steel surfaces shall be abrasive blast-cleaned in accordance with SSPC-SP10/NACE No. 2 unless otherwise specified by the purchaser. The blast anchor pattern or profile depth shall be 1.5 mil to 4.0 mil(38 µm to 102 µm) measured in accordance with ASTM D4417.

Preheating

Pipe that has been cleaned shall be preheated at temperature less than 260℃, the heat source shall not contaminate the pipe surface.

Thickness

The coating powder shall be applied to the preheated pipe at a uniform cure-film thickness of not less than 12 mils(305μm) on the exterior or interior. The maximum thickness shall not exceed a nominal 16 mils(406μm) unless recommended by the manufacturer or specified by the pruchaser.

Optional epoxy performance testing

The purchaser may specify additional testing to establish epoxy performance. The following test procedures, all of which shall be performed on production pipe test rings, may be specified:
1. Cross-section porosity.
2. Interface porosity.
3. Thermal analysis (DSC).
4. Permanent strain (bendability).
5. Water soak.
6. Impact.
7. Cathodic disbondment test.


Product detail pictures:

High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard  – Spiral detail pictures

High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard  – Spiral detail pictures

High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard  – Spiral detail pictures


Related Product Guide:

Control the standard by the details, show the power by quality. Our business has strived to establish a highly efficient and stable team staff and explored an effective good quality regulate course of action for High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard – Spiral , The product will supply to all over the world, such as: Morocco, Rome, Karachi, Our business activities and processes are engineered to make sure our customers have access to widest range of products with the shortest supply time lines. This achievement is made possible by our highly skilled and experienced team. We look for people who want to grow with us around the globe and stand out from the crowd. We now have people who embrace tomorrow, have vision, love stretching their minds and going far beyond what they thought was achievable.
  • This is the first business after our company establish, products and services are very satisfying, we have a good start, we hope to cooperate continuous in the future!
    5 Stars By Riva from Panama - 2018.09.19 18:37
    Speaking of this cooperation with the Chinese manufacturer, I just want to saywell dodne, we are very satisfied.
    5 Stars By Hellyngton Sato from Australia - 2017.03.07 13:42
    Write your message here and send it to us