We stick with the theory of quality first, company first, steady improvement and innovation to satisfy the customers for the management and zero defect, zero complaints as the quality objective. To perfect our provider, we deliver the items together with the fantastic good quality at the reasonable value for Steel Pipe Thickness , X52 SSAW Line Pipe Factories , Fbe Fusion Bonded Epoxy , We sincerely welcome close friends to barter company and start cooperation with us. We hope to affix hands with mates in different industries to make a excellent future.
Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral Detail:

Chemical Composition of ASTM A234 WPB & WPC

Element

Content, %

ASTM A234 WPB

ASTM A234 WPC

Carbon [C]

≤0.30

≤0.35

Manganese [Mn]

0.29-1.06

0.29-1.06

Phosphorus [P]

≤0.050

≤0.050

Sulfur [S]

≤0.058

≤0.058

Silicon [Si]

≥0.10

≥0.10

Chromium [Cr]

≤0.40

≤0.40

Molybdenum [Mo]

≤0.15

≤0.15

Nickel [Ni]

≤0.40

≤0.40

Copper [Cu]

≤0.40

≤0.40

Vanadium [V]

≤0.08

≤0.08

*The Carbon Equivalent [C.E.=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15] shall be no greater than 0.50 and shall be reported on MTC.

Mechanical Properties of ASTM A234 WPB & WPC

ASTM A234 Grades

Tensile Strength, min.

Yield Strength, min.

Elongation %, min

ksi

MPa

ksi

MPa

Longitudinal

Transverse

WPB

60

415

35

240

22

14

WPC

70

485

40

275

22

14

*1. WPB and WPC pipe fittings manufactured from plates shall have a minimum elongation of 17%.
*2. Unless required, hardness value doesn’t need to be reported.

Manufacture

The ASTM A234 carbon steel pipe fittings may be made from seamless pipes, welded pipes or plates by shaping operations of pressing, piercing, extruding, bending, fusion welding, machining, or by a combination of two or more these operations. All welds including welds in tubular products from which fittings are made shall be made in accordance with ASME Section IX. Post-weld heat treatment at 1100 to 1250°F[595 to 675°C] and radiographic examination shall be performed after the welding process.


Product detail pictures:

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures


Related Product Guide:

We always get the job done to be a tangible staff to ensure that we can easily offer you the best high-quality and the greatest value for Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral , The product will supply to all over the world, such as: Germany, Mauritius, Chicago, With all these supports, we can serve every customer with quality product and timely shipping with highly responsibility. Being a young growing company, we might not the best, but we are trying our best to be your good partner.
  • The company's products very well, we have purchased and cooperated many times, fair price and assured quality, in short, this is a trustworthy company!
    5 Stars By Johnny from New Zealand - 2018.11.06 10:04
    We are long-term partners, there is no disappointment every time, we hope to maintain this friendship later!
    5 Stars By Esther from Germany - 2017.12.09 14:01
    Write your message here and send it to us