Our pursuit and enterprise goal is to Always satisfy our customer requirements. We keep on to establish and style and design outstanding top quality goods for both our outdated and new prospects and realize a win-win prospect for our clientele likewise as us for Fbe Lined Pipe , Sewer Line , Gas Welding Exhaust Pipe , Our company is working by the operation principle of integrity-based, cooperation created, people oriented, win-win cooperation. We hope we can have a friendly relationship with businessman from all over the world.
Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral Detail:

Chemical Composition of ASTM A234 WPB & WPC

Element

Content, %

ASTM A234 WPB

ASTM A234 WPC

Carbon [C]

≤0.30

≤0.35

Manganese [Mn]

0.29-1.06

0.29-1.06

Phosphorus [P]

≤0.050

≤0.050

Sulfur [S]

≤0.058

≤0.058

Silicon [Si]

≥0.10

≥0.10

Chromium [Cr]

≤0.40

≤0.40

Molybdenum [Mo]

≤0.15

≤0.15

Nickel [Ni]

≤0.40

≤0.40

Copper [Cu]

≤0.40

≤0.40

Vanadium [V]

≤0.08

≤0.08

*The Carbon Equivalent [C.E.=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15] shall be no greater than 0.50 and shall be reported on MTC.

Mechanical Properties of ASTM A234 WPB & WPC

ASTM A234 Grades

Tensile Strength, min.

Yield Strength, min.

Elongation %, min

ksi

MPa

ksi

MPa

Longitudinal

Transverse

WPB

60

415

35

240

22

14

WPC

70

485

40

275

22

14

*1. WPB and WPC pipe fittings manufactured from plates shall have a minimum elongation of 17%.
*2. Unless required, hardness value doesn’t need to be reported.

Manufacture

The ASTM A234 carbon steel pipe fittings may be made from seamless pipes, welded pipes or plates by shaping operations of pressing, piercing, extruding, bending, fusion welding, machining, or by a combination of two or more these operations. All welds including welds in tubular products from which fittings are made shall be made in accordance with ASME Section IX. Post-weld heat treatment at 1100 to 1250°F[595 to 675°C] and radiographic examination shall be performed after the welding process.


Product detail pictures:

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures


Related Product Guide:

Our personnel are always inside the spirit of continuous improvement and excellence, and together with the outstanding excellent goods, favorable price and good after-sales services, we try to gain every customer's trust for Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral , The product will supply to all over the world, such as: Malaysia, Berlin, Islamabad, The president and all the company members would like to provide qualified goods and services for customers and sincerely welcome and cooperate with all native and foreign customers for a bright future.
  • The company has a good reputation in this industry, and finally it tured out that choose them is a good choice.
    5 Stars By Joa from Juventus - 2017.05.02 11:33
    We feel easy to cooperate with this company, the supplier is very responsible, thanks.There will be more in-depth cooperation.
    5 Stars By Judy from Nigeria - 2017.08.18 11:04
    Write your message here and send it to us