We always continually offer you by far the most conscientious customer service, and the widest variety of designs and styles with finest materials. These attempts include the availability of customized designs with speed and dispatch for High-Quality Seam Pipe , S235 J0 Spiral Steel Pipe Suppliers , Steel Pipe For Sale , If you are interested within our products and solutions, you should come to feel absolutely free to ship us your inquiry. We sincerely hope to ascertain win-win company relationships with you.
Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral Detail:

Chemical Composition of ASTM A234 WPB & WPC

Element

Content, %

ASTM A234 WPB

ASTM A234 WPC

Carbon [C]

≤0.30

≤0.35

Manganese [Mn]

0.29-1.06

0.29-1.06

Phosphorus [P]

≤0.050

≤0.050

Sulfur [S]

≤0.058

≤0.058

Silicon [Si]

≥0.10

≥0.10

Chromium [Cr]

≤0.40

≤0.40

Molybdenum [Mo]

≤0.15

≤0.15

Nickel [Ni]

≤0.40

≤0.40

Copper [Cu]

≤0.40

≤0.40

Vanadium [V]

≤0.08

≤0.08

*The Carbon Equivalent [C.E.=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15] shall be no greater than 0.50 and shall be reported on MTC.

Mechanical Properties of ASTM A234 WPB & WPC

ASTM A234 Grades

Tensile Strength, min.

Yield Strength, min.

Elongation %, min

ksi

MPa

ksi

MPa

Longitudinal

Transverse

WPB

60

415

35

240

22

14

WPC

70

485

40

275

22

14

*1. WPB and WPC pipe fittings manufactured from plates shall have a minimum elongation of 17%.
*2. Unless required, hardness value doesn’t need to be reported.

Manufacture

The ASTM A234 carbon steel pipe fittings may be made from seamless pipes, welded pipes or plates by shaping operations of pressing, piercing, extruding, bending, fusion welding, machining, or by a combination of two or more these operations. All welds including welds in tubular products from which fittings are made shall be made in accordance with ASME Section IX. Post-weld heat treatment at 1100 to 1250°F[595 to 675°C] and radiographic examination shall be performed after the welding process.


Product detail pictures:

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures


Related Product Guide:

We also provide item sourcing and flight consolidation solutions. We have now our very own manufacturing facility and sourcing place of work. We could provide you with nearly every kind of merchandise associated to our merchandise variety for Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral , The product will supply to all over the world, such as: Mauritania, Nicaragua, Albania, As an experienced group we also accept customized order and make it same as your picture or sample specifying specification and customer design packing. The main goal of our company is to build up a satisfactory memory to all customers, and establish a long term win-win business relationship. Choose us, we always wait for your appearance!
  • Managers are visionary, they have the idea of mutual benefits, continuous improvement and innovation, we have a pleasant conversation and Cooperation.
    5 Stars By Rigoberto Boler from Slovenia - 2017.11.11 11:41
    After the signing of the contract, we received satisfactory goods in a short term, this is a commendable manufacturer.
    5 Stars By Josephine from Guinea - 2017.02.28 14:19
    Write your message here and send it to us