We not only will try our greatest to present fantastic expert services to each purchaser, but also are ready to receive any suggestion offered by our prospects for Fbe Lining , S235 J0 Spiral Steel Pipe Factories , Steel Pipes And Fittings , We are sincerely looking forward to cooperate with customers all over the world. We believe we can satisfy with you. We also warmly welcome customers to visit our factory and purchase our products.
Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral Detail:

Chemical Composition of ASTM A234 WPB & WPC

Element

Content, %

ASTM A234 WPB

ASTM A234 WPC

Carbon [C]

≤0.30

≤0.35

Manganese [Mn]

0.29-1.06

0.29-1.06

Phosphorus [P]

≤0.050

≤0.050

Sulfur [S]

≤0.058

≤0.058

Silicon [Si]

≥0.10

≥0.10

Chromium [Cr]

≤0.40

≤0.40

Molybdenum [Mo]

≤0.15

≤0.15

Nickel [Ni]

≤0.40

≤0.40

Copper [Cu]

≤0.40

≤0.40

Vanadium [V]

≤0.08

≤0.08

*The Carbon Equivalent [C.E.=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15] shall be no greater than 0.50 and shall be reported on MTC.

Mechanical Properties of ASTM A234 WPB & WPC

ASTM A234 Grades

Tensile Strength, min.

Yield Strength, min.

Elongation %, min

ksi

MPa

ksi

MPa

Longitudinal

Transverse

WPB

60

415

35

240

22

14

WPC

70

485

40

275

22

14

*1. WPB and WPC pipe fittings manufactured from plates shall have a minimum elongation of 17%.
*2. Unless required, hardness value doesn’t need to be reported.

Manufacture

The ASTM A234 carbon steel pipe fittings may be made from seamless pipes, welded pipes or plates by shaping operations of pressing, piercing, extruding, bending, fusion welding, machining, or by a combination of two or more these operations. All welds including welds in tubular products from which fittings are made shall be made in accordance with ASME Section IX. Post-weld heat treatment at 1100 to 1250°F[595 to 675°C] and radiographic examination shall be performed after the welding process.


Product detail pictures:

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures


Related Product Guide:

Assume full responsibility to satisfy all needs of our clients; achieve continual advancements by endorsing the expansion of our purchasers; turn into the final permanent cooperative partner of clientele and maximize the interests of clients for Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral , The product will supply to all over the world, such as: Moldova, Costa rica, Sierra Leone, Today, We are with great passion and sincerity to further fulfill our global customers' needs with good quality and design innovation. We fully welcome customers from all over the world to establish stable and mutually beneficial business relationships, to have a bright future together.
  • The company has rich resources, advanced machinery, experienced workers and excellent services, hope you keep improving and perfecting your products and service, wish you better!
    5 Stars By ron gravatt from Kuala Lumpur - 2017.12.02 14:11
    Adhering to the business principle of mutual benefits, we have a happy and successful transaction, we think we will be the best business partner.
    5 Stars By Gabrielle from Venezuela - 2017.06.29 18:55
    Write your message here and send it to us